Double Nozzles Spray Gun for Liquid Silver Chrome Skill NA015-16

  • Before chrome, make sure the primer is completely (100%)dry;
  • Process of chrome: Spray DI Water---Then Spray K---Wait 3 seconds, Then Spray DI Water---Then Spray A&B---Then Spray H---Then Spray DI Water---Air Dry;
  • The spraying of DI water after K, make sure the object is well cleaned and there is no residue of the K solution (this process is very critical, if there is K residue, the surface of the chrome object will become very dirty;
  • K solution need to prepare 24 hours before spray chrome, until you see the K solution becomes slightly green, then you can prepare A, B, S and start the chrome work;
  • DI Water TDS Value should be below 2, test with TDS meter;
  • After the process of spray H, DI Water and air Dry, then don't touch the objects with bare hands, keep the objects away from dust, oil, scratching etc.; ●After air dry, the chromed objects need to be dried completely before spray the varnish; 8.Prepare suitable quantity of chrome chemicals, too much preparation of chrome chemicals may cause waste

    Model No.

    NA015-16

    SPRAY DISTANSE

    150-310mm

    NOZZLE SIZE

    1,0/1,5/2,5mm

    AIR PRESSURE

    4,0~8,0BAR

    Air CONSUMPTION

    320ml/min

    PAINT OUTPUT

    150ml/min

    PATTERN WIDTH

    200mm

     

    Leave Your Message